TPV 3190-Sarlink Aging Resistant
Other Products
Colette Trading (Tianjin) Co., Ltd. specializes in the sale of TPV 3190-Sarlink aging resistance , which can replace ExxonMobil, with price advantages and regular inventory;
Teknor Apex (referred to as TA Company) TPV 3190-Sarlink aging resistance improves performance and flexibility
Sarlink Thermoplastic Vulcanizate (TPV) is the preferred solution for critical applications requiring excellent elasticity and long-term performance. With faster and more economical processing, Sarlink TPVs provide a sustainable alternative to thermoset rubber in sealing applications. The Sarlink portfolio has recently expanded to include styrenic TPEs, which introduce unique performance characteristics such as improved flow properties for more complex designs. While our competitors focus on one chemistry, at Teknor Apex we offer multiple chemistries under one brand, enabling us to recommend the most suitable solution for your specific application.
| TPV 3190-Sarlink aging resistance Molding method | Injection moldingExtrusion | |||
TPV 3190-Sarlink aging resistance Technical parameters
| Physical properties | Value/Unit | Test standard | Test conditions |
|---|---|---|---|
Density | 0.94 g/cm³ | ASTM D792 | |
Shrinkage | |||
Longitudinal (Flow) | 1.6 % | Internal | 3mm thickness |
Transverse (Across Flow) | 1.3 % | Internal | 3mm thickness |
| Mechanical properties | Value/Unit | Test standard | Test conditions |
Tensile strength | |||
At 100% elongation | 7.1 Mpa | ASTM D 412 | Cross direction |
At 100% elongation | 7.9 Mpa | ASTM D 412 | Flow direction |
- | 13.5 Mpa | ASTM D 412 | Cross direction |
- | 11.5 Mpa | ASTM D 412 | Flow direction |
Tensile elongation | |||
Break (brk) | 746 % | ASTM D 412 | Cross direction |
Break (brk) | 570 % | ASTM D 412 | Flow direction |
Tear strength | 64 kN/m | ASTM D 624 | Unnicked, Cross direction |
Compression set | 62 % | ASTM D 395 | 125℃, 70Hrs |
Compression set | 37 % | ASTM D 395 | 23℃, 22Hrs |
Compression set | 53 % | ASTM D 395 | 70℃, 22Hrs |
| Impact properties | Value/Unit | Test standard | Test conditions |
Brittleness temperature | -59 °C | ISO 812 | |
| Hardness properties | Value/Unit | Test standard | Test conditions |
Shore hardness A | 90 A | ASTM D 2240 | 5sec, Extruded sample |
Shore hardness A | 93 A | ASTM D 2240 | 5sec, Injection molded sample |
| Flammability properties | Value/Unit | Test standard | Test conditions |
UL flame rating | |||
HB | - mm | UL94 | |
| Aging properties | Value/Unit | Test standard | Test conditions |
Hardness (thermal aging) | 0 - | ASTM D573 | Change, 135℃, 1000Hrs |
Hardness (thermal aging) | 2 - | ASTM D573 | Change, 150℃, 168Hrs |
Tensile strength (thermal aging) | 95 % | ASTM D573 | Retention, 135℃, 1000Hrs |
Tensile strength (thermal aging) | 93 % | ASTM D573 | Retention, 150℃, 168Hrs |
Elongation (thermal aging) | 88 % | ASTM D573 | Retention, 135℃, 1000Hrs |
Elongation (thermal aging) | 81 % | ASTM D573 | Retention, 150℃, 168Hrs |
Volume change | 73 % | ASTM D471 | ASTM Oil# |
| Industry Category | Rubber-Plastics |
|---|---|
| Product Category | |
| Brand: | Sarlink |
| Spec: | TPV 3190-Sarlink |
| Stock: | 5000 |
| Manufacturer: | |